Mechanical Properties Metric English Comments
Tensile Strength, Yield 485 - 515 MPa
70300 - 74700 psi
T direction
ArcelorMittal Speed 35-440 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..