Material Notes:
ASTM F-75 Cobalt Chromium alloys are widely used in orthopedic implants such as cemented total hip or knee arthroplasty as well as in metal-on-metal bearings in total hip arthroplasty. The alloys feature medium strength and stiffness combined with high corrosion resistance and good biocompatibility.Information provided by Stratasys®
Mechanical Properties Metric English Comments
Hardness, Rockwell C 34
34
Tensile Strength, Ultimate 896 MPa
130000 psi
Rm
Tensile Strength, Yield 600 MPa
87000 psi
Rp 0.2
Elongation at Break 10 %
10 %
Component Elements Properties Metric English Comments
Aluminum, Al 0.050 %
0.050 %
Carbon, C 0.30 %
0.30 %
Chromium, Cr 28.5 %
28.5 %
Cobalt, Co 63.315 %
63.315 %
Iron, Fe 0.20 %
0.20 %
Magnesium, Mg 0.50 %
0.50 %
Molybdenum, Mo 6.0 %
6.0 %
Nickel, Ni 0.25 %
0.25 %
Nitrogen, N 0.15 %
0.15 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.70 %
0.70 %
Sulfur, S 0.0050 %
0.0050 %
Titanium, Ti 0.010 %
0.010 %
Tungsten, W 0.010 %
0.010 %
Users viewing this material also viewed the following: