Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%)

Category Ceramic , Carbide
Manufacturer Anderman Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent thermal shock properties when in contact with molten metal. Available as tube, sheath, or rod up to 7.2 ft (2.2 m) long with diameters 0.6" to 4.7".Information provided by Anderman Ceramics.
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
Open Porosity 25 %
25 %
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 7.00 W/m-K

@Temperature 20.0 - 100 °C
48.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1400 °C
2550 °F
Component Elements Properties Metric English Comments
Al2O3 19 %
19 %
SiC 70 %
70 %
SiO2 10.5 %
10.5 %
Descriptive Properties Value Comments
Thermal Shock Resistance Very Good