Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast ADHESIET A Dry Air-Setting Refractory Mortar Description: Adhesiet A is a general purpose air setting mortar, supplied as a dry powder for use up to 1400°C.Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. .. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics 26 Insulation Bricks-ASTM Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics HH 40D Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics REFCAST Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics HH HG Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics HICCS Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | No Load |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | No Load |
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2) Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Du-Co Ceramics S-470 Aluminum Silicate Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Chosun Refractories CFS-1 Ceramic Foam Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
Chosun Refractories CT-140 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
Chosun Refractories PT-140 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
BNZ Materials BNZP-26A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%) Excellent thermal shock properties when in contact with molten metal. Available as tube, sheath, or rod up to 7.2 ft (2.2 m) long with diameters 0.6" to 4.7".Information provided by Anderman Cerami.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec 965 Toughened Alumina (Al2O3-ZrO2) Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |