Material Notes:
>Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Sintered properties below were determined using transverse rupture bars. Information provided by Ametek Specialty Metal Products.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 550 MPa
79800 psi
Elongation at Break 6.0 %
6.0 %
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 17 %
17 %
Iron, Fe 81 %
81 %
as balance
Manganese, Mn 0.20 %
0.20 %
Molybdenum, Mo 1.0 %
1.0 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.90 %
0.90 %
Sulfur, S 0.020 %
0.020 %