Material Notes:
Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness. Availability: Latin America, North America and South AmericaAdditive:Antiblock: NoSlip: NoProcessing Aid: YesThermal Stabilizer: YesApplications:Food packagingForm Fill and Seal PackagingHeavy Duty BagsLamination FilmMultilayer Packaging FilmShrink FilmStand Up Pouches Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ExxonMobil method
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 17.2 MPa
2500 psi
ASTM D882
Film Tensile Strength at Yield, TD 19.3 MPa
2800 psi
ASTM D882
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 810 %
810 %
ASTM D882
Puncture Energy 2.49 J
1.83 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 20 g
20 g
ASTM D1922
Elmendorf Tear Strength TD 610 g
610 g
ASTM D1922
Dart Drop Test <= 80.0 g
<= 0.176 lb
ASTM D1709
Film Tensile Strength at Break, MD 57.9 MPa
8400 psi
ASTM D882
Film Tensile Strength at Break, TD 47.6 MPa
6900 psi
ASTM D882
1% Secant Modulus, MD 427 MPa
62000 psi
ASTM D882
1% Secant Modulus, TD 517 MPa
75000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 254 °C
<= 489 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 14 %
14 %
ASTM D1003
Gloss 40 %
40 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 11 lbf
ExxonMobil Method
Users viewing this material also viewed the following: