Physical Properties Metric English Comments
Density 0.655 g/cc

@Temperature 180 °C
0.0237 lb/in³

@Temperature 356 °F
0.790 g/cc

@Temperature 160 °C
0.0285 lb/in³

@Temperature 320 °F