Polymer Property : Density = 0.0285 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.790 g/cc

@Temperature 160 °C
0.0285 lb/in³

@Temperature 320 °F
Akzo Nobel Extrusion of MDPE with 0.65% Expancel E930-120