Accuratus Accuflect™ Light-Reflecting Ceramic

Category Ceramic , Glaze
Manufacturer Accuratus Ceramic
Trade Name Accuflect™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Accuratus Accuflect™ Light-Reflecting Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: Highly diffuse reflectance from near UV to InfraredTypical Uses: Flashlamp pumped solid state laser cavities, Diode laser pumped solid state laser cavities, High temperature diffuse illumination, High temperature lamp housings, Tube furnace radiant energy reflectorsGeneral Information: B6 type Accuflect™ is a porous ceramic usable to 1300 °C. B6 material has enhanced reflectance in the infrared. When the material is used in water cooled cavities or areas of significant contamination a glazed ceramic designated G6 is recommended. G6 is usable to 750 °C.Accuflect™ reflects 95% to 99% of incident light from 450 nm to 2500 nm. The reflectivity is essentially non-specular with nearly perfect LAMBERTIAN behavior across the entire spectrum.Accuflect™ is available in two product types. The B6 material has the virgin ceramic surface produced during manufacture. The G6 material has a specialty clear glaze applied to seal the surface porosity of the virgin material, allow easy cleaning and provide a non-contaminating surface where it is exposed to atmosphere or liquid environments.Information provided by Accuratus.
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Porosity 30 %
30 %
Mechanical Properties Metric English Comments
Flexural Strength 27.5 MPa
3990 psi
Compressive Strength 62.0 MPa
8990 psi
Thermal Properties Metric English Comments
CTE, linear 7.70 µm/m-°C
4.28 µin/in-°F
Thermal Conductivity 5.80 W/m-K
40.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1200 °C
2190 °F
no load
Electrical Properties Metric English Comments
Dielectric Constant 5.5
5.5
Dielectric Strength 3.00 kV/mm
76.2 kV/in
Dissipation Factor 0.0030
0.0030
Descriptive Properties Value Comments
Color White