Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 62.0 MPa | 8990 psi | Perpendicular to pressing direction |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Compressive Strength | 62.0 MPa | 8990 psi | Practical Use; ASTM-D695 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 62.0 MPa | 8990 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 62.0 MPa | 8990 psi | |
Accuratus Accuflect™ Light-Reflecting Ceramic Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: .. |
|||
Compressive Strength | 62.0 MPa | 8990 psi | |
Henkel SynCore 9823.1 Syntactic Film Toughened, low density syntactic core, superior moisture resistance, co-curable with a variety of 250°F / 121°C curing epoxy prepregs. |