Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.0 MPa | 2750 psi | 2 in/min; ASTM D638 |
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | >= 19.0 MPa | >= 2750 psi | ASTM D412 Method A |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D638 |
Teknor Apex APEX® 3600-80NT Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D638 |
Teknor Apex APEX® 586 Polyvinyl Chloride, Flexible Notes: 60°C Insulation; RoHS Compliant Uses: Tubing; Wire JacketingForms: Pellets Wire Types: SPT-1; SPT-2 Agency Ratings: UL 498; UL 62 Processing Method: Injection Molding Additional Informatio.. |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D638 |
Teknor Apex APEX® 84842-B Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: High Heat Resistance; Sunlight Resistant (720 hours) Uses: Wire and Cable Applications; Wire JacketingAgency Ratings: UL 62; UL QMTT2 .E73402 Forms: .. |
|||
Tensile Strength at Break | >= 19.0 MPa | >= 2750 psi | ASTM D412 Method A |
Seals Eastern 7182B Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D638 |
Teknor Apex APEX® 65012 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D638 |
Chesterton ARC I BX1 Impact & Wear Resistant Epoxy Composite Description: An advanced grade epoxy and urethane composite for the repair and protection of all metal surfaces subjected to severe abrasion and impact. It is normally applied at a thickness of 6 mm.. |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D412 |
Compuestos Dominicanos Polycom VG-410180 PVC Compound Other flexible extrusion compounds are polycom VG which can be used to manufacture garden hoses of high gloss, clarity and outdoor resistance.Applications: Garden hose extrusion Appearance: Clear gr.. |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | |
Abatron AboWeld 8104-13 Polysulfide-Epoxy Sealant and Caulk AboWeld 8104-13 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It has high hardness and rigidity, very low elongation, and is often used with sand or o.. |
|||
Tensile Strength at Break | 19.0 MPa | 2750 psi | ASTM D412 |
Compuestos Dominicanos Polycom VY-310585 PVC Compound The Polycom VY series are compounds for the extrusion of both stripes for chaise lounge and flexible window sidings with outstanding weather and outdoors resistance. Also, in the VY series the are .. |