Abatron AboCast 8503-10/AboCure 8503-10 5-Minute Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8503-10/AboCure 8503-10 5-Minute Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 8503-10/AboCure 8503-10 is a very-fast-hardening 2-component epoxy adhesive, casting, and patching compound. It is the toughest, most machineable, 5-minute metal-filled putty available. It has the superior tooling, adhesive, and structural properties required in machine shops, the metal-working industry, and maintenance applications. It is neither an electrical conductor nor magnetic. It does not have the brittleness typical of conventional 5-minute epoxies. It also provides high resistance to weather, water, salt spray, alkalis, diluted acids, several fuels, solvents, and other chemicals. Unlike other epoxies, a thin layer of this compound does not need any longer to harden than a thick casting.
Physical Properties Metric English Comments
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
Mechanical Properties Metric English Comments
Hardness, Shore D 13

@Time 601 sec
13

@Time 0.167 hour
40

@Time 1800 sec
40

@Time 0.500 hour
68

@Time 3600 sec
68

@Time 1.00 hour
76

@Time 86400 sec
76

@Time 24.0 hour
Shear Strength 14.5 MPa
2100 psi
Tensile lap
Processing Properties Metric English Comments
Pot Life 5.0 min
5.0 min
Gel Time 5.00 min

@Thickness 1.27 mm
5.00 min

@Thickness 0.0500 in
Descriptive Properties Value Comments
Color Gray
Parts by Weight (pbw) 100
AboCast 8503-10
100
AboCure 8503-10
Viscosity Putty