Aaron Industries AAROPRENE® ATPR 1000 50A Elastomeric Compound

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® ATPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® ATPR 1000 50A Elastomeric Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Melt Flow 90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
"E"; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 47 - 53
47 - 53
ASTM D2240
Tensile Strength 5.31 MPa
770 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Tensile Modulus 0.00193 GPa
0.280 ksi
ASTM D412
Tear Strength 31.0 kN/m
177 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 345
345
H-18; ASTM D1044