Mechanical Properties Metric English Comments
Tear Strength 31.0 kN/m
177 pli
post cured- 4 hours at 204°C; Die B
Multibase SILASTIC® C7-4550 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 31.0 kN/m
177 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 52A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 31.0 kN/m
177 pli
Die B
Momentive Performance Materials Siloprenâ„¢ FFSL 7041 Fully Fluorinated Liquid Silicone Rubber
This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe..
Tear Strength 31.0 kN/m
177 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LIM 6030 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tear Strength 31.0 kN/m
177 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 52A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 31.0 kN/m
177 pli
73°F, Die C, Across Flow; ASTM D624
ExxonMobil Santoprene® 121-85M100 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Tear Strength 31.0 kN/m
177 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770P Highly Extended Low-Cost Hose
FormulationNordel® IP 4770P
Tear Strength 31.0 kN/m
177 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose
FormulationNordel® IP 4770R
Tear Strength 31.0 - 48.0 kN/m
177 - 274 pli
ASTM D 624
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Tear Strength 31.0 kN/m
177 pli
Die C; ASTM D624
Aaron Industries AAROPRENE® ATPR 1000 50A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Tear Strength 31.0 kN/m
177 pli
Perpendicular to flow; ISO 34-B
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer
Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Tear Strength 31.0 kN/m
177 pli
ISO 34-B
AlphaGary Evoprene™ 091 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tear Strength 31.0 kN/m
177 pli
ISO 34-B
AlphaGary Evoprene™ GC 5690 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..