ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age

Category Metal , Ferrous Metal , Maraging Steel
Manufacturer ATI Allvac
Trade Name VascoMax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 459
459
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 504
504
Estimated from Rockwell C value.
Hardness, Rockwell C 48
48
Hardness, Vickers 482
482
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1759 MPa
255100 psi
Tensile Strength, Yield 1690 MPa

@Strain 0.200 %
245000 psi

@Strain 0.200 %
Elongation at Break 12 %
12 %
Reduction of Area 50 %
50 %
Component Elements Properties Metric English Comments
Aluminum, Al 0.10 %
0.10 %
Carbon, C 0.020 %
0.020 %
Cobalt, Co 7.8 %
7.8 %
Iron, Fe 69 %
69 %
as balance
Manganese, Mn 0.050 %
0.050 %
Molybdenum, Mo 4.8 %
4.8 %
Nickel, Ni 18 %
18 %
Phosphorous, P 0.0050 %
0.0050 %
Silicon, Si 0.050 %
0.050 %
Sulfur, S 0.0050 %
0.0050 %
Titanium, Ti 0.40 %
0.40 %