Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1759 MPa | 255100 psi | Hardened 1900°F, Tempered 400°F |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 1759 MPa | 255100 psi | Hardened 1900°F, Tempered 800°F |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 1759 MPa | 255100 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 427°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Tensile Strength, Ultimate | 1759 MPa | 255100 psi | |
ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts. |
|||
Tensile Strength, Ultimate | 1759 MPa | 255100 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |