Material Notes:
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as there are no VOC emissions from adhesives and, as the components are not made from a range of incompatible materials, they are more easily recycled at the end of their useful life. The over-molding process can be used in highly technical applications such as components for the automotive industry, shells and casings for power tools, parts for domestic appliances, and seals which can be molded directly onto the frame.Information provided by A.P.I. SpA
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Median; ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 32

@Time 15.0 sec
32

@Time 0.00417 hour
Median; ASTM D 2240
Tensile Strength 4.00 MPa
580 psi
ASTM D 638
Elongation at Break 620 %
620 %
ASTM D 638
100% Modulus 0.00120 GPa
0.174 ksi
ASTM D 638
300% Modulus 0.00200 GPa
0.290 ksi
ASTM D 638
Tear Strength 17.0 kN/m
97.0 pli
ASTM D 624
Compression Set 26 %

@Temperature 23.0 °C,
Time 259000 sec
26 %

@Temperature 73.4 °F,
Time 72.0 hour
ASTM D 395
70 %

@Temperature 70.0 °C,
Time 86400 sec
70 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D 395
85 %

@Temperature 100 °C,
Time 86400 sec
85 %

@Temperature 212 °F,
Time 24.0 hour
ASTM D 395
Descriptive Properties Value Comments
Compatibility ABS
ASA
PA12
PC
PET
PMMA
PVC
SAN
TPU
Food contact On Request
Hygroscopicity Slightly
Main Features Very Soft
Ozone Aging Resistance Excellent
72h, 40°C, 200 ppcm, Tension = 20%
Processing Injection Molding
Weathering Good