Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00120 GPa | 0.174 ksi | ISO/R527 |
Polykemi AB POLYelast TPE EZ506X Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00120 - 0.00200 GPa | 0.174 - 0.290 ksi | DIN 53504 S2 |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ISO 37 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Extrusion, Pebble Gray Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ISO 37 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Injection Molding, Pebble Gray Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | MSZ ISO 527 |
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ISO 37 |
AlphaGary Evoprene™ 047 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE
features excellent so.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ASTM D 638 |
API Megol AM DP2392/32 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5655 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00120 GPa | 0.174 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |