Esstech X-852-0000 FIT 852 Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-852-0000 FIT 852 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FIT 852 Resin is a novel low shrink urethane monomer based on Esstech's proprietary methacrylate technology. FIT possesses a volumetric shrinkage of 2.0 - 2.5% and conversion of 65 - 80% without filler.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Viscosity 78000 cP

@Temperature 40.0 °C
78000 cP

@Temperature 104 °F
790000 cP

@Temperature 25.0 °C
790000 cP

@Temperature 77.0 °F
Optical Properties Metric English Comments
Refractive Index 1.4941
1.4941
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Acidity (% Methacrylic Acid) < 0.3
MeHQ Inhibitor (ppm) 3500