Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1025

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Precipitation Hardening Stainless
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1025.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, low-temperature heat treatments minimize distortion and scaling. This alloy is widely used in the aerospace, chemical, petrochemical, food processing, paper and general metalworking industries. The material supplied from the mill is in Condition A. After fabrication eight standard heat treatments have been developed to provide a wide range of properties.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Typical
Mechanical Properties Metric English Comments
Hardness, Rockwell C 38
38
Tensile Strength, Ultimate 1276 MPa
185100 psi
Tensile Strength, Yield 1172 MPa

@Strain 0.200 %
170000 psi

@Strain 0.200 %
Elongation at Break 8.0 %
8.0 %
in 2 inches
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 15 - 17.5 %
15 - 17.5 %
Copper, Cu 3.0 - 5.0 %
3.0 - 5.0 %
Iron, Fe 69.91 - 78.85 %
69.91 - 78.85 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Nb + Ta 0.15 - 0.45 %
0.15 - 0.45 %
Nickel, Ni 3.0 - 5.0 %
3.0 - 5.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Copyright © lookpolymers.com All Rights Reserved