Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypel® PEHD.7/.962 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Entec Engineered Resins
Trade Name Hypel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypel® PEHD.7/.962 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec
Physical Properties Metric English Comments
Specific Gravity 0.964 g/cc
0.964 g/cc
ASTM D792
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
Unannealed; ASTM D648
Vicat Softening Point 129 °C
264 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525