Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1276 MPa
185100 psi
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1025
AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Cold-Worked Full hard
AK Steel 201 Austenitic Stainless steel
AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Cold-Worked Full hard
AK Steel 201LN Austenitic Stainless steel
AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Cold-Worked Full hard
AK Steel 301 Austenitic Stainless steel
AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Tensile Strength, Ultimate 1276 MPa
185100 psi
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Tensile Strength, Ultimate 1276 MPa
185100 psi
ATI Allvac® Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Data provided by Allvac.Applications: Turbine discs and shafts, compressor blades and discs, high-temperature bolting, high-temperature devices, cryogenics.
Tensile Strength, Ultimate 1276 MPa
185100 psi
ATI Allegheny Ludlum AL 13-8™ H 1025 Precipitation Hardening Alloy
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..
Tensile Strength, Ultimate >= 1276 MPa
>= 185100 psi
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Tensile Strength, Ultimate 1276 MPa
185100 psi
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Data provided by Allvac.Applications: Turbine compressor blades and discs, shafts, spacers, fasteners, miscellaneous jet engine hardware; space shuttle turbo pump seals.Waspaloy is a registered trad..
Copyright © lookpolymers.com All Rights Reserved