Material Notes:
QLE 1035 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: 100% solids Long open time Excellent adhesion Tough, resilient coatingPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
"B" component
1.34 g/cc
1.34 g/cc
"A" component
Viscosity 800 cP
800 cP
"B" component
18000 cP
18000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
cured 20 mins @150°C
Tensile Strength, Yield 1.40 MPa
203 psi
cured 20 mins @150°C
Elongation at Break 200 %
200 %
cured 20 mins @150°C
Processing Properties Metric English Comments
Gel Time 1380 min
1380 min
Descriptive Properties Value Comments
Color Clear
"B" component
White
"A" component