Polymer Property : Tensile Strength, Yield = 203 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.40 MPa
203 psi
ASTM D638
Premix Thermoplastics PRESEAL® TPE 5020
General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o..
Tensile Strength, Yield 1.40 MPa
203 psi
ISO 37
Premix Thermoplastics PRESEAL® TPE 5020
General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o..
Tensile Strength, Yield 1.40 MPa
203 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength, Yield >= 1.40 MPa
>= 203 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5243 Neoprene / Chloroprene
General purpose neopreneInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 1.40 MPa
203 psi
at 100% elongation, maximum
Dow Corning SILASTIC® 37085-V SILICONE RUBBER BLACK
50 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning
Tensile Strength, Yield 1.40 MPa
203 psi
ACC MM903 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Tensile Strength, Yield 1.40 MPa
203 psi
cured 20 mins @150°C
ACC QLE 1035 QSI Quantum Silicones 38 Durometer Addition Cure Elastomer for Coating
QLE 1035 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: ..