Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00050 - 0.0010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.00050 - 0.0010 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.00050 - 0.0010 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.00050 - 0.0010 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Linear Mold Shrinkage | 0.00030 - 0.0010 cm/cm | 0.00030 - 0.0010 in/in | |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |
|||
Linear Mold Shrinkage | -0.00200 - 0.0010 cm/cm | -0.00200 - 0.0010 in/in | processing, expansion/shrinkage; ISO 2577 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |