A. Schulman PAPERMATCH® T-39617 Specialty Masterbatch

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PAPERMATCH® T-39617 Specialty Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPAPERMATCH® T-39617 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. This masterbatch is a white, medium opacity grade with a smooth surface finish. PAPERMATCH® T-39617 provides good print quality with low die lip build up. PAPERMATH® T-39617 is typically recommended for use at 50% in polypropylene cast film applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 51 %
51 %
ASTM D2765
Descriptive Properties Value Comments
Moisture 500
ppm, ASTM D789 @ 190°C
Pellet Count 35
pellets/gram