3M Tartan™ 200 Making Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Tartan™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Tartan™ 200 Making Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A utility purpose paper tape used for holding, bundling, sealing, non-critical masking and a vast number of other jobs where a pressure-sensitive tape is needed.Information provided by 3M
Physical Properties Metric English Comments
Thickness 140 microns
5.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 250 MPa
36300 psi
ASTM D3756
Elongation at Break 8.0 %
8.0 %
ASTM D3756
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Natural colored crepe paper
Users viewing this material also viewed the following: