3M Scotchrap™ 50 Tape

Category Polymer , Tape , Thermoplastic , Vinyl (PVC)
Manufacturer 3M
Trade Name Scotchrap™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchrap™ 50 Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings and joints on all mill-coated pipe and electrical conduit systems. These tapes are: Resistant to salt water, soil acids, alkalies and salts, common chemicals, chemical vapors, and exposure to outdoor weathering and sunlight. Resistant to impact, abrasions, punctures, and tears. Tape 50 is a highly conformable, all-weather 10 mil (0.254 mm) thick tape designed for application over a wide temperature range.Information provided by 3M
Physical Properties Metric English Comments
Water Vapor Transmission 15.5 g/m²/day
0.998 g/100 in²/day
ASTM D3833
Thickness 254 microns
10.0 mil
ASTM D1000
Mechanical Properties Metric English Comments
Elongation at Break 100 %

@Temperature -12.0 °C
100 %

@Temperature 10.4 °F
ASTM D1000
200 %

@Temperature 23.0 °C
200 %

@Temperature 73.4 °F
ASTM D1000
Peel Strength 0.219 kN/m

@Temperature 23.0 °C
1.25 pli

@Temperature 73.4 °F
Adhesion to Steel; ASTM D1000
0.219 kN/m

@Temperature 23.0 °C
1.25 pli

@Temperature 73.4 °F
Adhesion to Backing; ASTM D1000
0.3287 kN/m

@Temperature -12.0 °C
1.875 pli

@Temperature 10.4 °F
Adhesion to Steel; ASTM D1000
0.3287 kN/m

@Temperature -12.0 °C
1.875 pli

@Temperature 10.4 °F
Adhesion to Backing; ASTM D1000
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.6 °C
150 °F
Application
80.0 °C
176 °F
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
-12.0 °C
10.4 °F
Application
Electrical Properties Metric English Comments
Dielectric Breakdown >= 12000 V
>= 12000 V
ASTM D1000
Processing Properties Metric English Comments
Moisture Content 0.30 %
0.30 %
ASTM D570
Descriptive Properties Value Comments
Appearance Black