Thermal Properties Metric English Comments
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Non-brittle after 3 minutes
Precision Polymer Engineering E70Z Ethylene Propylene Rubber
Peroxide cured, grey Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electri..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Recommended
Nye Lubricants 791B (RL) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Sundex 790
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Silpruf® Construction Sealant
One-part, for weatherseals, structural glazing, and general purpose sealing. Cure Method: Alkoxy (Neutral). Tack-free time 5 to 10 hr.; Peel Strength 55 lb/in.; Sag/slump 0.1 in.Data provided by the..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Elasticity is retained to this temperature.
Momentive Performance Materials UltraPruf® SCS 2300 Construction Sealant
One-part, for concrete, masonry, and stone. Matte finish. Cure Method: Alkoxy (Neutral); Tack-free time 5 to 10 hr. Peel Strength 55 lb/in. Sag/slump 0.1 in.Data provided by the manufacturer, GE..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Cumar P-10
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Sundex 790
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
JIS-K-6723
Denka REOMER G G5048 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
JIS-K-6723
Denka REOMER G G5059 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
JIS-K-6723
Denka REOMER G G8053 Thermoplastic Elastomer, For Injection Molding
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
3M Scotchrap™ 50 Tape
3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
3M Scotchrap™ 51 Tape
3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Elasticity is retained to this temperature.
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant
High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..
Minimum Service Temperature, Air -48.0 °C
-54.4 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Cumar P-10