3M Scotch® 8626 Tear Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 8626 Tear Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Tear Tape 8624 is a designed for use as the easy-opening device on paperboard and light- to medium-weight corrugated fiberboard packaging materials. Typical easy-opening applications for Scotch® Tape 8626 include: overnight courier envelopes; overnight courier boxes; audio/video/CD/book mailers; printed boxes used in the retail market for such items as electronics, toys, medical, computers, and clothing; and shipping boxes used by catalogs and “mail order” retailers, who want to avoid product damage from knives, razor blades and scissors used to open the packages.Information provided by 3M
Physical Properties Metric English Comments
Thickness 157 microns
6.20 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.5 MPa
3560 psi
ASTM D3759
Elongation at Break 30 %
30 %
ASTM D3759
Peel Strength 0.82172 kN/m
4.6875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Ivory