Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 157 microns | 6.20 mil | |
Hexcel® HexForce™ 1526 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 157 microns | 6.20 mil | |
Hexcel® HexForce™ 7627 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 157 microns | 6.20 mil | Liner |
3M 9671LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 157 microns | 6.20 mil | Liner |
3M 9672LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 157 microns | 6.20 mil | Liner 83# Polycoated kraft ) |
3M 8132LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 157 microns | 6.20 mil | Liner 83# Polycoated kraft ) |
3M 8153LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 157 microns | 6.20 mil | Caliper |
3M 9475LE High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Thickness | 157 microns | 6.20 mil | ASTM D3652 |
3M Scotch® 8626 Tear Tape Scotch® Tear Tape 8624 is a designed for use as the easy-opening device on paperboard and light- to medium-weight corrugated fiberboard packaging materials. Typical easy-opening applications for Sc.. |
|||
Thickness | 157 microns | 6.20 mil | Liner |
3M 9653LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 157 microns | 6.20 mil | Liner Caliper |
3M 9832HL Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |