3M FC-1100 Acid Mist Suppressant

Category Fluid , Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FC-1100 Acid Mist Suppressant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Acid Mist Suppressant FC-1100 is a fluorochemical additive that provides outstanding sulfuric acid mist suppression in the copper electrowinning tankhouse without the formation of a stable foam blanket at the surface of the electrowinning cell. FC-1100 suppressant can significantly reduce tankhouse acid mist levels when used alone or in conjunction with mechanical barriers, such as polypropylene macrospheres, with no adverse effects to either the solvent extraction or electrowinning processInformation provided by 3M
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Solids Content 45 - 55 %
45 - 55 %
Fluorochemical
Viscosity <= 100 cP
<= 100 cP
Surface Tension 35 dynes/cm
35 dynes/cm
30 ppm
40 dynes/cm
40 dynes/cm
14 ppm
45 dynes/cm
45 dynes/cm
6 ppm
50 dynes/cm
50 dynes/cm
1 ppm
Processing Properties Metric English Comments
Moisture Content 45 - 55 %
45 - 55 %
Descriptive Properties Value Comments
Color Light Amber
Form Liquid