Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ Fluorel™ FT-2430 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Fluorel™ FT-2430 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosphonium Accelerator. Improved elongation retention after long-term heat aging. Improved acid and organic solvent resistance. Blend with incorporated cure gums; coatings. Used in Raw Gums.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
Mooney Viscosity 30

@Temperature 121 °C
30

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Tensile Strength, Ultimate 13.0 MPa
1890 psi
Tensile Strength, Yield 2.30 MPa
334 psi
M100
Elongation at Break 255 %
255 %
Coefficient of Friction, Dynamic 0.80
0.80
Compression Set 38 %

@Temperature 200 °C
38 %

@Temperature 392 °F
70 hr; ASTM D395B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -14.0 °C
6.80 °F
TR10