Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.30 MPa | 334 psi | M100 |
3M Dyneon™ Fluorel™ FT-2430 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phospho.. |
|||
Tensile Strength, Yield | 2.30 MPa @Strain 100 % |
334 psi @Strain 100 % |
|
Daikin DAI-EL G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Extrusion of hose and tubing, etc.Information provided by Daikin Indus.. |
|||
Tensile Strength, Yield | 2.30 MPa @Strain 100 % |
334 psi @Strain 100 % |
|
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie.. |
|||
Tensile Strength, Yield | 2.30 MPa | 334 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5403 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |