Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ Fluorel™ FE-5840Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Fluorel™ FE-5840Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.1%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the cleanest running Dyneon O-ring grade polymers available; provide excellent mold release & improved scorch safety. This allows molding at higher temperatures (>200°C) for faster cure cycles - resulting in parts with improved dimensional stability. FE-5621Q and FE-5641Q have lower mold shrinkage. Used in O-Ring and molded goods applications.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
Mooney Viscosity 37

@Temperature 121 °C
37

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
Tensile Strength, Ultimate 14.0 MPa
2030 psi
Tensile Strength, Yield 6.80 MPa
986 psi
M100
Elongation at Break 210 %
210 %
Coefficient of Friction, Dynamic 0.80
0.80
Compression Set 26 %

@Temperature 200 °C
26 %

@Temperature 392 °F
70 hr; ASTM D395B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -7.00 °C
19.4 °F
TR10
Users viewing this material also viewed the following: