3M 6143 Heavy Duty Water Activated Paper Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 6143 Heavy Duty Water Activated Paper Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Heavy Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornstarch based adhesive system.Information provided by 3M
Physical Properties Metric English Comments
Thickness 191 microns
7.50 mil
Caliper; ASTM D645
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 200 g
200 g
ASTM D1922
Elmendorf Tear Strength TD 225 g
225 g
ASTM D1922
Film Tensile Strength at Break, MD 53.3 MPa
7730 psi
ASTM D5803