Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 53.3 MPa
7730 psi
ASTM D5803
3M 6143 Heavy Duty Water Activated Paper Tape
3M™ Heavy Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornstar..