Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 225 g
225 g
ASTM D 1922
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che..
Elmendorf Tear Strength TD 225 g
225 g
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade
DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl..
Elmendorf Tear Strength TD 225 g
225 g
ASTM D1922
3M 6143 Heavy Duty Water Activated Paper Tape
3M™ Heavy Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornstar..