3M 2510 Black Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2510 Black Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Black Masking Tape 2510 is a general purpose masking tape for holding, bundling, sealing and general paint masking where dark colored tape is required.Information provided by 3M
Physical Properties Metric English Comments
Thickness 3.56 microns
0.140 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D3759
Elongation at Break 9.0 %
9.0 %
ASTM D3759
Peel Strength 0.38347 kN/m
2.1875 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
for up to 60 mins, removed cleanly
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Black