Polymer Property : Volume Resistivity = 30000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity >= 30000 ohm-cm

@Temperature 20.0 °C
>= 30000 ohm-cm

@Temperature 68.0 °F
IEC 672-1
CeramTec CD 101 Silicon Carbide, SiC-ZrB2
CD101 is a zirconia reinforced silicon carbide designed for maximum hardness.