Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 30000 ohm-cm @Temperature 20.0 °C |
>= 30000 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |