Electrical Properties Metric English Comments
Volume Resistivity 4.20e+16 ohm-cm
4.20e+16 ohm-cm
Tra-Con Tra-Cast F353 Optically Opaque Casting System
TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical..