Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.20e+16 ohm-cm | 4.20e+16 ohm-cm | |
Tra-Con Tra-Cast F353 Optically Opaque Casting System TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical.. |