Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
Pyrotek TS-84 Thermoset Electrical Insulation Product (Nema Grade: XX)
Paper reinforcement, Phenolic Resin, Natural/Black Color. Good insulation in dry or humid conditions.Information provided by Pyrotek.
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
XX Phenolic Laminate
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b..
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
Conditioned; IEC 60093
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber
PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
ASTM D247
Plenco 4300 Phenolic, Granular, Transfer Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..