Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4300 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Cellulose Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4300 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electrical control applications. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04300 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.163 %
0.163 %
ASTM D570
Linear Mold Shrinkage 0.0042 cm/cm
0.0042 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 0.66 %
0.66 %
ASTM D638
Tensile Modulus 10.0 GPa
1450 ksi
ASTM D638
Flexural Strength 92.0 MPa
13300 psi
ASTM D790
Flexural Modulus 9.40 GPa
1360 ksi
ASTM D790
Compressive Strength 172 MPa
24900 psi
ASTM D695
Poissons Ratio 0.33
0.33
ASTM D638
Shear Modulus 3.76 GPa
545 ksi
Calculated
Izod Impact, Notched 0.202 J/cm
0.378 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.215 J/cm²
1.02 ft-lb/in²
ASTM D256
Impact 92
92
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 194 °C
381 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 33 %
33 %
ASTM D2863
Shrinkage 0.158 %
0.158 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
ASTM D247
Dielectric Constant 5.7
5.7
ASTM D150
Dielectric Strength 12.0 kV/mm
305 kV/in
Short Time; ASTM D149
Dissipation Factor 0.058
0.058
ASTM D150
Arc Resistance 182 sec
182 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved