Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided by Aurora Technologies.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
Tensile Strength, Ultimate 93.1 MPa
13500 psi
Flexural Strength 117 MPa
17000 psi
Compressive Strength 207 MPa
30000 psi
Shear Strength 68.9 MPa
10000 psi
Izod Impact, Notched 0.294 J/cm
0.550 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
Mechanical
140 °C
284 °F
Electrical
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
Surface Resistance 4.00e+10 ohm
4.00e+10 ohm
Dielectric Constant 4.6

@Frequency 1e+6 Hz
4.6

@Frequency 1e+6 Hz
Dielectric Strength 19.7 kV/mm
500 kV/in
Dielectric Breakdown 60000 V
60000 V
Dissipation Factor 0.040

@Frequency 1e+6 Hz
0.040

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Color Natural/Black