Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.30e+14 ohm-cm | 3.30e+14 ohm-cm | 70°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hb Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Volume Resistivity | 3.30e+14 ohm-cm | 3.30e+14 ohm-cm | |
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning |