Material Notes:
Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.980 g/cc

@Temperature 25.0 °C
0.970 - 0.980 g/cc

@Temperature 77.0 °F
Viscosity <= 440 cP
<= 440 cP
dynamic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Volume Resistivity 3.30e+14 ohm-cm
3.30e+14 ohm-cm
Dielectric Constant 2.6

@Frequency 100 Hz
2.6

@Frequency 100 Hz
2.61

@Frequency 100000 Hz
2.61

@Frequency 100000 Hz
Dielectric Strength 17.3 kV/mm
440 kV/in
Dissipation Factor <= 0.00020

@Frequency 100000 Hz
<= 0.00020

@Frequency 100000 Hz
0.021

@Frequency 100 Hz
0.021

@Frequency 100 Hz
Processing Properties Metric English Comments
Cure Time 2.50 min

@Temperature 125 °C
0.0417 hour

@Temperature 257 °F
480 - 660 min

@Temperature 22.0 °C
8.00 - 11.0 hour

@Temperature 71.6 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance translucent
Color green
Flowable yes
Self Leveling yes
Water Resistant yes
Working Time (min) >60
Users viewing this material also viewed the following: