Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+13 - 3.00e+13 ohm-cm | 1.00e+13 - 3.00e+13 ohm-cm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |