Polymer Property : Volume Resistivity = 2.70e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+11 ohm-cm

@Temperature 50.0 °C
2.70e+11 ohm-cm

@Temperature 122 °F
ASTM D257
Teknor Apex APEX® 87-L101F-3 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Volume Resistivity 2.70e+11 ohm-cm

@Temperature 50.0 °C
2.70e+11 ohm-cm

@Temperature 122 °F
ASTM D257
Teknor Apex APEX® 01-A0383A-85 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Volume Resistivity 2.70e+11 ohm-cm
2.70e+11 ohm-cm
ASTM D247
Plenco 7476 Phenolic, Granular, Transfer Molded
PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. ..
Volume Resistivity 2.70e+11 ohm-cm
2.70e+11 ohm-cm
ASTM D247
Plenco 2000 Phenolic, Granular, Transfer Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..